Saturday, February 25, 2012

Aerospace Aluminium Alloys in Aircraft Skins

Aerospace Aluminium Alloys in Aircraft Skins

High strength aluminium alloys.

The origin of aluminium alloys in aircraft construction started with the first practical all-metal aircraft in 1915 made by Junkers in Germany, of materials said to be `iron and steel'. Steel presented the advantages of a high modulus of elasticity, high proof stress and high tensile strength. Unfortunately these were accompanied by a high specific gravity, almost three times that of the aluminium alloys and about ten times that of plywood. Aircraft designers during the 1930s were therefore forced to use steel in its thinnest forms. To ensure stability against buckling of the thin plate, intricate shapes for spar sections were devised.

In 1909 Alfred Wilm, in Germany, accidentally discovered that an aluminium alloy containing 3.5 per cent copper, 0.5 per cent magnesium and silicon and iron, as unintended impurities, spontaneously hardened after quenching from about 480°C. The patent rights of this material were acquired by Durener Metallwerke who marketed the alloy under the name Duralumin. For half a century this alloy has been used in the wrought heat-treated, naturally aged condition. The improvements in these properties produced by artificial ageing at a raised temperature of, for example, 175°C, were not exploited in the aircraft industry until about 1934.

In addition to the development of duralumin (first used as a main structural material by Junkers in 1917) three other causes contributed to the replacement of steel by aluminium alloys. These were a better understanding of the process of heat treatment, the introduction of extrusions in a wide range of sections and the use of pure aluminium cladding to provide greater resistance to corrosion. By 1938, three groups of aluminium alloys dominated the field of aircraft construction and, in fact, they retain their importance to the present day. The groups are separated by virtue of their chemical composition, to which they owe their capacity for strengthening under heat treatment.

The first group is contained under the general name duralumin having a typical composition of: 4 per cent copper, 0.5 per cent magnesium, 0.5 per cent manganese, 0.3 per cent silicon, 0.2 per cent iron, with the remainder aluminium. The naturally aged version was covered by Air Ministry Specification DTD 18 issued in 1924, while artificially aged duralumin came under Specification DTD 111 in 1929. DTD 111 provided for slight reductions in 0.1 per cent proof stress and tensile strength.

The second group of aluminium alloys differs from duralumin chiefly by the introduction of 1 to 2 per cent of nickel, a high content of magnesium and possible variations in the amounts of copper, silicon and iron. `Y' alloy, the oldest member of the group, has a typical composition of. 4 per cent copper, 2 per cent nickel, 1.5 cent magnesium, the remainder being aluminium and was covered by Specification DTD 58A issued in 1927. Its most important property was its retention of strength at high temperatures, which meant that it was a particularly suitable material for aero engine pistons. Its use in airframe construction has been of a limited nature only. Research by Rolls-Royce and development by High Duty Alloys Ltd produced the `RR' series of alloys. Based on Y alloy, the RR alloys had some of the nickel replaced by iron and the copper reduced. One of the earliest of these alloys, RR56 had approximately half of the 2 per cent nickel replaced by iron, the copper content reduced from 4 to 2 per cent, and was used for forgings and extrusions in aero engines and airframes.

The third and latest group depends upon the inclusion of zinc and magnesium and their high strength. Covered by Specification DTD 363 issued in 1937, these alloys had a nominal composition: 2.5 per cent copper, 5 per cent zinc, 3 per cent magnesium and up to 1 per cent nickel. In modern versions of this alloy nickel has been eliminated and provision made for the addition of chromium and further amounts of manganese.

Aircraft structural aluminium.

Of the three basic structural materials, namely wood, steel and aluminium alloy, only wood is no longer of significance except in laminates for non-structural bulkheads, floorings and furnishings. Most modern aircraft still rely on modified forms of the high strength aerospace aluminium alloys which were introduced during the early part of the 20th century. Steels are used where high strength, high stiffness and wear resistance are required. Other materials, such as titanium and fibre-reinforced composites first used about 1950, are finding expanding uses in airframe construction.

Friday, February 17, 2012

Aircraft and Aerospace Aluminum Alloys

Aircraft and Aerospace Aluminum Alloys

Pure aluminum and pure magnesium are completely unsuitable as structural materials for airframes, because they have very low strength. However, when alloyed (chemically mixed) with each other or with other metals, their strength is vastly improved, and they form the most widely used group of airframe materials. Alloying metals include zinc, copper, manganese, silicon and lithium, and may be used singly or in combination.

There are very many different variations, each having different properties and so suited to different uses. Magnesium alloys are very prone to attack by sea water, and their use in carrier-based aircraft is generally avoided. Aluminum alloys, although denser than magnesium alloys, are much less prone to chemical attack, and are cheaper, so are more widely used. 2024 alloy, known as duralumin, consists of 93.5 percent aluminum, 4.4 percent copper, 1.5 percent manganese and 0.6 per cent magnesium, and is the most widely used of all materials in aircraft structures. Aluminum alloys are more prone to corrosion than pure aluminum, so pure aluminum is often rolled onto the surfaces of its alloys to form a protective layer. The process is known as cladding, and sheets of alloy treated like this are known as clad sheets or Al-clad. Another common means of protecting aluminum alloys is anodising - conversion of the surface layer to a form which is more corrosion-resistant by an electro-chemical process. Aluminum-lithium alloys are superior to aluminum-zinc and aluminum-copper alloys in strength and stiffness, so can be used to save weight. Their use is limited because they are around three times as expensive.

An interesting property which certain aluminum alloys share with titanium is that they can be super-plastically formed (SPF). When the material is heated to a certain temperature, far below its melting point, it is capable of being stretched by several times its own length without tearing or local thinning. It can then be deformed, using an inert gas such as argon, to fill a mould and take its shape exactly, with no spring-back when the pressure is released. There are various techniques based on this property, which can be used to make extremely complicated shapes accurately and with minimum weight. The high initial cost of tooling means SPF is limited to certain high-cost items, and it is not yet suited to mass production. Items such as pressure vessels, small tanks and reservoirs may be made using this technique.

Advantages of aluminum and magnesium alloys

1. High strength-to-weight ratios
2. A wide range of different alloys, to suit a range of different uses
3. Low density, so greater bulk for same weight means they can be used in a greater thickness than denser materials, and thus are less prone to local buckling; this applies to magnesium alloys even more than aluminum alloys
4. Available in many standard forms - sheet, plate, tube, bar, extrusions
5. Aluminum alloys are easy to work after simple heat treatment
6. Can be super-plastically formed (certain aluminum alloys only)

Disadvantages

1. Prone to corrosion, so need protective finishes, particularly magnesium alloys
2. Many alloys have limited strength, especially at elevated temperatures
3. Magnesium alloys have low strength (but high strength-to-weight ratio)
4. No fatigue limit (see section on fatigue later in this chapter)